In ChinaK232 material is Age hardening type iron base alloy.
Chemical composition of K232, K232 mechanical properties, K232 datasheet, K232 equivalent grade, Heat treatment and temperature process of K232.
| C | Max 0.15 |
| Si | Max 0.5 |
| Mn | Max 0.5 |
| P | Max 0.02 |
| S | Max 0.015 |
| Cr | 12.0-16.0 |
| Ni | 38.0-42.0 |
| Mo | 1.50-2.50 |
| W | 3.50-4.50 |
| B | Max 0.02 |
| Al | 1.80-2.30 |
| Ti | 2.30-2.80 |
| other | Ce:Max 0.02,ZrMax 0.05 |
| Rp0.2 (MPa) | 957 (≥) |
| Rm (MPa) | 399 (≥) |
| AKV (J) | 43 |
| A (%) | 33 |
| Z (%) | 43 |
| Hardness | HBW 313 |
| K232 Round bar: | 1mm-800mm |
| K232 Square bar: | 10mm * 10mm-600mm *600mm |
| K232 Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
| K232 Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
| K232 Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
| K232 Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |