In ChinaK417 material is Age hardening type Nickel base alloy.
Chemical composition of K417, K417 mechanical properties, K417 datasheet, K417 equivalent grade, Heat treatment and temperature process of K417.
C | 0.13-0.22 |
Si | Max 0.5 |
Mn | Max 0.5 |
P | Max 0.015 |
S | Max 0.01 |
Cr | 8.50-9.50 |
Ni | Balance |
Mo | 2.50-3.50 |
V | 0.60-0.90 |
Co | 14.0-16.0 |
B | 0.012-0.022 |
Al | 4.80-5.70 |
Ti | 4.50-5.00 |
other | Zr :0.05-0.09 |
Rp0.2 (MPa) | 988 (≥) |
Rm (MPa) | 735 (≥) |
AKV (J) | 32 |
A (%) | 44 |
Z (%) | 14 |
Hardness | HBW 333 |
K417 Round bar: | 1mm-800mm |
K417 Square bar: | 10mm * 10mm-600mm *600mm |
K417 Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
K417 Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
K417 Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |