Certified Company
DNV&ABSCertified Company
DNV&ABSCertified Company
ISO 9001:2008R&D Production
In ChinaK438 material is Age hardening type Nickel base alloy.
Chemical composition of K438, K438 mechanical properties, K438 datasheet, K438 equivalent grade, Heat treatment and temperature process of K438.
| C | 0.10-0.20 |
| Si | Max 0.5 |
| Mn | Max 0.5 |
| P | Max 0.015 |
| S | Max 0.01 |
| Cr | 15.5-16.5 |
| Ni | Balance |
| Mo | 1.50-2.00 |
| W | 2.40-2.80 |
| Co | 8.00-9.00 |
| B | 0.005-0.015 |
| Nb | 0.50-1.10 |
| Al | 3.20-3.70 |
| Ti | 3.00-3.50 |
| Ta | 1.50-2.00 |
| other | Zr:0.05-0.15 |
| Rp0.2 (MPa) | 921 (≥) |
| Rm (MPa) | 941 (≥) |
| AKV (J) | 41 |
| A (%) | 23 |
| Z (%) | 42 |
| Hardness | HBW 432 |
| K438 Round bar: | 1mm-800mm |
| K438 Square bar: | 10mm * 10mm-600mm *600mm |
| K438 Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
| K438 Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
| K438 Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
| K438 Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |