In China03XH28MДT material is Russia GOCT standard deformation of high temperature alloy grades and chemical composition.
Chemical composition of 03XH28MДT, 03XH28MДT mechanical properties, 03XH28MДT datasheet, 03XH28MДT equivalent grade, Heat treatment and temperature process of 03XH28MДT.
03XH28MДT |
C: | Max | 0.03 |
Si: | Max | 0.80 |
Mn: | Max | 0.80 |
P: | Max | 0.035 |
S: | Max | 0.020 |
Cr: | 22.00 | 25.00 |
Ni: | 26.00 | 29.00 |
Mo: | 2.50 | 3.00 |
Al: | Max | Min |
Ti: | 0.50 | 0.90 |
Fe: | Max | Min |
Cu: | 2.50 | 3.50 |
Rp0.2 (MPa) | 163 (≥) |
Rm (MPa) | 889 (≥) |
AKV (J) | 22 |
A (%) | 11 |
Z (%) | 43 |
Hardness | HBW 141 |
03XH28MДT Round bar: | 1mm-800mm |
03XH28MДT Square bar: | 10mm * 10mm-600mm *600mm |
03XH28MДT Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
03XH28MДT Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
03XH28MДT Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
03XH28MДT Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |