In ChinaXH75MБTЮ material is Russia GOCT standard deformation of high temperature alloy grades and chemical composition.
Chemical composition of XH75MБTЮ, XH75MБTЮ mechanical properties, XH75MБTЮ datasheet, XH75MБTЮ equivalent grade, Heat treatment and temperature process of XH75MБTЮ.
XH75MБTЮ |
C: | Max | 0.10 |
Si: | Max | 0.80 |
Mn: | Max | 0.40 |
P: | Max | 0.020 |
S: | Max | 0.012 |
Cr: | 19.00 | 22.00 |
Ni: | Max | remaining |
Mo: | 1.80 | 2.30 |
Al: | 0.35 | 0.75 |
Ti: | 0.35 | 0.75 |
Fe: | Max | 3.00 |
Nb: | 0.90 | 1.30 |
Rp0.2 (MPa) | 479 (≥) |
Rm (MPa) | 435 (≥) |
AKV (J) | 12 |
A (%) | 22 |
Z (%) | 12 |
Hardness | HBW 111 |
XH75MБTЮ Round bar: | 1mm-800mm |
XH75MБTЮ Square bar: | 10mm * 10mm-600mm *600mm |
XH75MБTЮ Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
XH75MБTЮ Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
XH75MБTЮ Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
XH75MБTЮ Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |