In China08X10H20T2 material is Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition.
Chemical composition of 08X10H20T2, 08X10H20T2 mechanical properties, 08X10H20T2 datasheet, 08X10H20T2 equivalent grade, Heat treatment and temperature process of 08X10H20T2.
08X10H20T2 |
C: | Max | 0.08 |
Si: | Max | 0.80 |
Mn: | Max | 2.00 |
P: | Max | 0.035 |
S: | Max | 0.030 |
Cr: | 10.00 | 12.00 |
Ni: | 18.00 | 20.00 |
Mo: | Max | 0.30 |
W: | Max | 0.20 |
Ti: | 1.50 | 2.50 |
Al: | Max | 1.00 |
Rp0.2 (MPa) | 199 (≥) |
Rm (MPa) | 319 (≥) |
AKV (J) | 13 |
A (%) | 23 |
Z (%) | 33 |
Hardness | HBW 431 |
08X10H20T2 Round bar: | 1mm-800mm |
08X10H20T2 Square bar: | 10mm * 10mm-600mm *600mm |
08X10H20T2 Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
08X10H20T2 Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
08X10H20T2 Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
08X10H20T2 Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |