In ChinaHR53 material is B.S. BS 2HR 53 (2010) Specification for nickel-iron-chromium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 42.5, Cr 12.5, Mo 5.8, Ti 3.0, Fe remainder) B.S. BS HR 53 Specification for nickel-iron-chromium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 42.5, Cr 12.5, Mo 5.8, Ti 3.0, Fe remainder) Specification for nickel-iron-chromium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 42.5, Cr 12.5, Mo 5.8, Ti 3.0, Fe remainder).
Chemical composition of HR53, HR53 mechanical properties, HR53 datasheet, HR53 equivalent grade, Heat treatment and temperature process of HR53.
B.S. BS 2HR 53 (2010) Specification for nickel-iron-chromium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 42.5, Cr 12.5, Mo 5.8, Ti 3.0, Fe remainder) |
B.S. BS HR 53 Specification for nickel-iron-chromium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 42.5, Cr 12.5, Mo 5.8, Ti 3.0, Fe remainder) |
HR53 |
C: | 0.02 | 0.06 |
Si: | Max | 0.40 |
Mn: | Max | 0.50 |
P: | Max | 0.020 |
S: | Max | 0.020 |
Cr: | 11.00 | 14.00 |
Ni: | 40.00 | 45.00 |
Mo: | 5.00 | 6.50 |
Co: | Max | 1.00 |
Ti: | 2.80 | 3.10 |
Fe: | Max | remaining |
Al: | Max | 0.30 |
Cu: | Max | 0.20 |
B: | 0.010 | 0.020 |
Pb: | Max | 0.0010 |
Bi: | Max | 0.0001 |
Ag: | Max | 0.0005 |
Rp0.2 (MPa) | 624 (≥) |
Rm (MPa) | 357 (≥) |
AKV (J) | 33 |
A (%) | 43 |
Z (%) | 22 |
Hardness | HBW 234 |
HR53 Round bar: | 1mm-800mm |
HR53 Square bar: | 10mm * 10mm-600mm *600mm |
HR53 Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
HR53 Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
HR53 Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
HR53 Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |