Certified Company
DNV&ABSCertified Company
DNV&ABSCertified Company
ISO 9001:2008R&D Production
In ChinaNCF 750 material is JIS G 4902 (1991) Corrosion-resisting and heat-resisting superalloy plates and sheets Corrosion-resisting and heat-resisting superalloy plates and sheets.
Chemical composition of NCF 750, NCF 750 mechanical properties, NCF 750 datasheet, NCF 750 equivalent grade, Heat treatment and temperature process of NCF 750.
C: | Max | 0.08 |
Si: | Max | 0.50 |
Mn: | Max | 1.00 |
P: | Max | 0.03 |
S: | Max | 0.015 |
Cr: | 14.00 | 17.00 |
Ni: | 70.00 | Min |
Cu: | Max | 0.50 |
Al: | 0.40 | 1.00 |
Ti: | 2.25 | 2.75 |
Fe: | 5.00 | 9.00 |
Nb+Ta: | 0.70 | 1.20 |
Rp0.2 (MPa) | 778 (≥) |
Rm (MPa) | 775 (≥) |
AKV (J) | 14 |
A (%) | 14 |
Z (%) | 42 |
Hardness | HBW 241 |
NCF 750 Round bar: | 1mm-800mm |
NCF 750 Square bar: | 10mm * 10mm-600mm *600mm |
NCF 750 Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
NCF 750 Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
NCF 750 Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
NCF 750 Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |