In ChinaNCF751 material is KS D 3531 (2007) Corrosion - resisting and heat - resisting superalloy bars KS D 3532 (2002) Corrosion - resisting and heat - resisting superalloy plates and sheets Corrosion - resisting and heat - resisting superalloy plates and sheets.
Chemical composition of NCF751, NCF751 mechanical properties, NCF751 datasheet, NCF751 equivalent grade, Heat treatment and temperature process of NCF751.
KS D 3531 (2007) Corrosion - resisting and heat - resisting superalloy bars |
KS D 3532 (2002) Corrosion - resisting and heat - resisting superalloy plates and sheets |
C: | Max | 0.10 |
Si: | Max | 0.50 |
Mn: | Max | 1.00 |
P: | Max | 0.030 |
S: | Max | 0.015 |
Cr: | 14.00 | 17.00 |
Ni: | 70.00 | Min |
Cu: | Max | 0.50 |
Al: | 0.90 | 1.50 |
Ti: | 2.00 | 2.60 |
Fe: | 5.00 | 9.00 |
Nb+Ta: | 0.70 | 1.20 |
Rp0.2 (MPa) | 653 (≥) |
Rm (MPa) | 738 (≥) |
AKV (J) | 21 |
A (%) | 41 |
Z (%) | 13 |
Hardness | HBW 423 |
NCF751 Round bar: | 1mm-800mm |
NCF751 Square bar: | 10mm * 10mm-600mm *600mm |
NCF751 Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
NCF751 Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
NCF751 Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
NCF751 Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |