Certified Company
DNV&ABSCertified Company
DNV&ABSCertified Company
ISO 9001:2008R&D Production
In ChinaXH77TЮP material is Russia GOCT standard deformation of high temperature alloy grades and chemical composition.
Chemical composition of XH77TЮP, XH77TЮP mechanical properties, XH77TЮP datasheet, XH77TЮP equivalent grade, Heat treatment and temperature process of XH77TЮP.
C: | Max | 0.07 |
Si: | Max | 0.60 |
Mn: | Max | 0.40 |
P: | Max | 0.015 |
S: | Max | 0.007 |
Cr: | 19.00 | 22.00 |
Ni: | Max | remaining |
Mo: | Max | Min |
Al: | 0.60 | 1.00 |
Ti: | 2.40 | 2.80 |
Fe: | Max | 1.00 |
B: | Max | 0.010 |
Ce: | Max | 0.01 |
Rp0.2 (MPa) | 519 (≥) |
Rm (MPa) | 985 (≥) |
AKV (J) | 34 |
A (%) | 32 |
Z (%) | 12 |
Hardness | HBW 214 |
XH77TЮP Round bar: | 1mm-800mm |
XH77TЮP Square bar: | 10mm * 10mm-600mm *600mm |
XH77TЮP Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
XH77TЮP Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
XH77TЮP Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
XH77TЮP Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |