In ChinaWaspaloy material is AMS SAE AMS 5708K (2008) Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution Heat Treated Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution Heat Treated.
Chemical composition of Waspaloy, Waspaloy mechanical properties, Waspaloy datasheet, Waspaloy equivalent grade, Heat treatment and temperature process of Waspaloy.
AMS SAE AMS 5708K (2008) Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution Heat Treated |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
C: | Max | 0.07 |
Si: | Max | 0.10 |
Mn: | Max | 0.10 |
Cr: | Max | 19.75 |
Ni: | Max | remaining |
Mo: | Max | 4.45 |
Co: | Max | 14.00 |
W: | Max | Min |
Al: | Max | 1.40 |
Cu: | Max | Min |
Ti: | Max | 3.00 |
Fe: | Max | 0.75 |
B: | Max | 0.005 |
Zr: | Max | 0.04 |
Rp0.2 (MPa) | 838 (≥) |
Rm (MPa) | 586 (≥) |
AKV (J) | 12 |
A (%) | 11 |
Z (%) | 11 |
Hardness | HBW 333 |
Waspaloy Round bar: | 1mm-800mm |
Waspaloy Square bar: | 10mm * 10mm-600mm *600mm |
Waspaloy Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
Waspaloy Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
Waspaloy Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
Waspaloy Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |