In ChinaWaspaloy material is SAE SAE AMS 5709H (2008) Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution, Stabilization, and Precipitation Heat Treated Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution, Stabilization, and Precipitation Heat Treated.
Chemical composition of Waspaloy, Waspaloy mechanical properties, Waspaloy datasheet, Waspaloy equivalent grade, Heat treatment and temperature process of Waspaloy.
SAE SAE AMS 5709H (2008) Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution, Stabilization, and Precipitation Heat Treated |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
C: | Max | 0.07 |
Si: | Max | 0.10 |
Mn: | Max | 0.10 |
Cr: | Max | 19.75 |
Ni: | Max | remaining |
Mo: | Max | 4.45 |
Co: | Max | 14.00 |
W: | Max | Min |
Al: | Max | 1.40 |
Cu: | Max | Min |
Ti: | Max | 3.00 |
Fe: | Max | 0.75 |
B: | Max | 0.005 |
Zr: | Max | 0.04 |
Rp0.2 (MPa) | 174 (≥) |
Rm (MPa) | 426 (≥) |
AKV (J) | 42 |
A (%) | 24 |
Z (%) | 13 |
Hardness | HBW 432 |
Waspaloy Round bar: | 1mm-800mm |
Waspaloy Square bar: | 10mm * 10mm-600mm *600mm |
Waspaloy Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
Waspaloy Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
Waspaloy Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
Waspaloy Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |