In ChinaWaspaloy material is SAE SAE AMS 5706L (2008) Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated.
Chemical composition of Waspaloy, Waspaloy mechanical properties, Waspaloy datasheet, Waspaloy equivalent grade, Heat treatment and temperature process of Waspaloy.
SAE SAE AMS 5706L (2008) Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
Waspaloy |
C: | Max | 0.07 |
Si: | Max | 0.10 |
Mn: | Max | 0.10 |
Cr: | Max | 19.75 |
Ni: | Max | remaining |
Mo: | Max | 4.45 |
Co: | Max | 14.00 |
W: | Max | Min |
Al: | Max | 1.40 |
Cu: | Max | Min |
Ti: | Max | 3.00 |
Fe: | Max | 0.75 |
B: | Max | 0.005 |
Zr: | Max | 0.04 |
Rp0.2 (MPa) | 271 (≥) |
Rm (MPa) | 788 (≥) |
AKV (J) | 24 |
A (%) | 34 |
Z (%) | 34 |
Hardness | HBW 321 |
Waspaloy Round bar: | 1mm-800mm |
Waspaloy Square bar: | 10mm * 10mm-600mm *600mm |
Waspaloy Flat bar: | Thickness:8mm-800mm Width:10mm to 1500mm |
Waspaloy Sheet or Plate: | Thickness:3mm-80mm Width:1.5mm to 1500mm |
Waspaloy Strip or Coil: | Thickness:0.1mm-3mm Width:1.5mm-1500mm |
Waspaloy Forgings: | Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes |